Abstract
The causes and the influence factors of the defects of center porosity and secondary pipe of the casting superalloy ingot are briefly introduced, and the study on the principle and technical characters of grain refinement technology with dynamic methods carried out. The mechanism, working parameter and the test result of the typical application methods including the technologies of vibration of ultrasonic, the vibration of mould, the stir of mould and oscillation in the riser were investigated in detail. By comparing the advantages and disadvantages of different methods and also according to the practical production situation of our company, the most appropriate one for improving the defects of center porosity and secondary pipe is proposed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.