Abstract

The decomposition of tetraisopropyl orthotitanate (TTIP), a representative precursor used in the atomic layer deposition (ALD) of titanium dioxide (TiO2) film, and the resulting changes in the thin film properties of the TiO2 film were investigated. TTIP was evaluated after exposure to thermal stress in an enclosed container. The vapor pressure results provide reasonable evidence that impurities are generated by the decomposition of TTIP under thermal stress. These impurities led to changes in the thermal properties of TTIP and changes in the growth rate, morphology, and composition of the thin film; in particular, these impurities increased the unstable oxidation states of Ti2+ (TiO) content in the TiO2 film. The changes in the properties of the TiO2 film resulting from the changes in the physical properties of TTIP led to a change in the properties of the device. We proved that the thermal stability of the precursor is a factor that can determine the reliability of the ALD process and the resulting thin film. Additionally, systematic evaluation of the precursor can provide useful information that can improve the development of the precursor and the consistency of the process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.