A nitrogen-doped photocatalyst (N-TiO2) is prepared from 15% TiCl3 and 25% aqueous NH3 solution as precursor. The synthesised material is characterised by XRD, BET, TEM, DRS and XPS and is used for photocatalytic decolourisation of Metanil Yellow under visible-light illumination. The experimental parameters, viz, photocatalyst dose, initial dye concentration and solution pH influence the decolourisation process. At pH 3.5, N-TiO2 can decolourise almost 89% of the dye at equilibrium within 240 min. COD study reveals ∼92% mineralisation of the dye in 360 min of irradiation. The photocatalytic reaction is allowed to proceed only after the attainment of adsorption equilibrium between N-TiO2-Metanil Yellow. The adsorption is carried out by batch process under different experimental conditions, namely, N-TiO2 dose, initial dye concentration and solution pH. The adsorption process attains equilibrium within 60 min and follows Lagergren first-order kinetics. On the other hand, the photocatalytic decolourisation of Metanil Yellow is suitably fitted with the modified Langmuir–Hinselwood model. Modification of TiO2 improved the decolourisation of the dye by ∼8 times compared to TiO2 P25.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.