A hexabromobenzene (HBB, C6Br6) powder was subjected to co-grinding with excess CaO powder in air using a planetary ball mill to investigate mechanochemical debromination of the HBB sample. The reaction proceeds smoothly with an increase in both grinding time and molar ratio of CaO addition. The co-grinding enables us to debrominate HBB, forming CaBr2, C and CaCO3 besides excess CaO in the product. CaBr2 in the product tends to absorb moisture from the atmosphere to form CaBr2 x nH2O. The reaction yield is quantitatively evaluated by measuring the amount of water-soluble bromide through water washing and the amount of unreacted HBB through toluene washing. It is found that almost 100% of debromination is achieved by 6 h grinding with the molar ratio kept constant at 2:1. Radicals are detected in the ground products, possibly due to rupture in the covalent bonds of C-C and C-Br in HBB.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.