Abstract

In order to uniformly distribute SiCp in the aluminium matrix and prepare SiCp/Al composites with high mechanical and damping properties, a preparation method of colloidal dispersion and suction filtration was developed. It was observed from the microstructure of the composites that the SiCp/Al composites prepared by colloidal dispersion and suction filtration method had good interfacial structures, and the interfacial reaction between SiCp and aluminium matrix was effectively inhibited. Tensile mechanical properties at room temperature and damping properties in the temperature range of 25 °C to 300 °C were tested for the SiCp/Al composites with volume fractions of 5% to 10%. The results showed that SiCp/Al composites have excellent mechanical and damping properties when the volume fraction of SiCp was 7%. This is because SiCp were uniformly distributed in the aluminium matrix, and formed a good interfacial bond with the aluminium matrix, which benefitted both the interfacial slip loss and the strengthening effect of SiCp.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call