Abstract

Pb(Zr,Ti)O3 (PZT) thick films directly deposited onto stainless steel (SS) sheets by the aerosol deposition method were annealed by CO2 laser (CL) radiation. The surface brilliance of the SS sheets was not influenced by thermal heating and the temperature of the reverse side of the film (i.e., the SS sheet) was measured at 150°C or less. The remanent polarization, coercive field values, and the dielectric constant are 27.8 μC/cm2, 31.6 kV/cm, and 1366, respectively. The diffusion layer between the PZT and the SS sheet was minimized by the use of CL radiation compared with using an electric furnace.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.