Introduction: The purpose of this study was to compare the cyclic fatigue of different types of nickel-titanium rotary files at body temperature. Methods: Four types of rotary instruments with tip size 0.25 were used: HyFlex EDM (OneFile, variable taper, Colten/Whaledent), ProTaper Gold (F2, 0.08 taper, Dentsply), XP-endo Finisher (zero tapers, FKG Dentaire) and 2Shape (TS2, 0.06 taper, Micro-Mega). Ten files for each instrument were tested for cyclic fatigue at body temperature and rotated until fracture occurred in a simulated canal with an angle curvature of 60°, a radius curvature of 5 mm, and a canal width of 1.5 mm. Four groups were formed for all instruments (total number = 40). The number of cycles to fracture and the length of fractured fragment were recorded, and statistical analysis was completed using analysis of variance with significance at a (p-value < 0.05). Results: The cyclic fatigue resistance of the HyFlex EDM OneFile was significantly greater than the other instruments, while that of the 2Shape TS2 was significantly lower (p < 0.05). Conclusion: Within the limitations of this study, the HyFlex EDM OneFile was more resistant to cyclic fatigue than the XP-endo Finisher, ProTaper Gold F2 and 2Shape TS2 files

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.