Abstract
Thermoplastic elastomer vulcanizate (TPV) and liquid silicone rubber (LSR) are replacement candidates for ethylene-propylene-diene rubbers (EPDM), as they offer the possibility for two-component injection moulding. In this study, these material types were compared side by side in cyclic compression tests. The materials were also characterized to provide details on the formulations. Compared to the rubbers, the TPV had higher compression set (after a given cycle) and hysteresis loss, and a stronger Mullins effect. This is due to the thermoplastic matrix in the TPV. The LSR had lower compression set (after a given cycle) than the EPDM, but stronger Mullins effect and higher relative hysteresis loss. These differences between the LSR and the EPDM are likely due to differences in polymer network structure and type of filler. Methods for quantifying the Mullins effect are proposed, and correlations between a Mullins index and parameters such as compression set are discussed. The EPDMs showed a distinct trend in compression set, relative hysteresis loss and relaxed stress fraction vs. strain amplitude; these entities were almost independent of strain amplitude in the range 15–35%, while they increased in this range for the TPV and the LSR. The difference between the compression set values of the LSR and the EPDM decreased with increasing strain amplitude and increasing strain recovery time.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.