Abstract

We experimentally demonstrate the current-induced domain wall motion in [CoFe/Pt]5 nanowire with perpendicular magnetic anisotropy. By use of the scanning MOKE measurement, we observe that two domain walls are moved simultaneously by spin polarized current at the current density of 1.43 times 1012 A/m2. The domain wall speed is estimated to be about 1.5 m/s, determined by the domain wall displacement (750 nm) and the current pulse duration (500 ns). From in situ resistance measurement, the temperature of the nanowire rises up to 700 K when the domain wall moves at such the high current density.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.