Abstract

This paper reports the results of investigations carried out to determine the Curie temperature (Tc) of some annealed praseodymium-based alloys represented by the formula Pr14Fe79.9-xCoxB6Nb0.1. The Curie temperature of these permanent magnet alloys increase linearly with the cobalt content at about (10.2±0.3) oC/at%. Pr14Fe80B6 and Pr14Fe79.9B6Nb0.1 magnetic alloys with a Tc of 290oC have been used as a standard reference. Magnets were prepared from the alloys using the hydrogenation, disproportionation, desorption and recombination (HDDR) process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.