The effect of cure characteristics and hardness of LCr filled SMR L compound were investigated. The size of LCr were 20 25 mm in range. Six compounds; 0, 5, 15, 25, 35 and 50 per hundred rubber (phr) of LCr were prepared by using two roll mill at room temperature. Cure characteristics such as scorch time,t2, cure time,t90, minimum torque, ML, maximum torque, MH, and cure rate index (CRI), and hardness of LCr filled SMR L were examined using rheometer. Result indicated that, all results for t2, t90, ML and MH shows the decrease with increasing in filler loading. CRI shows the increasing value with increasing LCr loading. Hardness, Ha value increase slightly with increasing LCr loading.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.