We report the fabrication of the Cu–Ni–Zr–Ti bulk amorphous alloys by warm rolling of amorphous powders, which have been prepared by a high-pressure gas atomization. The Cu 54Ni 6Zr 22Ti 18 amorphous powders obtained by a high-pressure He gas atomization method has a wide supercooled liquid region of 53 K. By warm rolling of amorphous powders in the supercooled liquid state, a fully amorphous Cu 54Ni 6Zr 22Ti 18 alloy is successfully synthesized. The conditions for rolling are obtained from the time–temperature–transformation curve by measuring the time for the onset of crystallization during isothermal annealing in differential scanning calorimetry. The rolled bulk amorphous Cu 54Ni 6Zr 22Ti 18 alloy exhibited high strength about 1.9 GPa, which is against similar to that obtained in the as-cast bulk amorphous alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.