Abstract

This article shows the results of fabricating a device through vacuum deposition by synthesizing a perovskite thin film in the powder form. Light emitting diodes (LEDs) were fabricated using a single-source and host-dopant system of the perovskite produced in the powder form. Both CsPbBr3 and Cs4PbBr6 used in the host-dopant system were green, and the host was tris(8-quinolinolato) aluminum(III). It is confirmed that the display efficiency and optical characteristics are significantly improved by the dopant ratio. The 3%-doped CsPbBr3 based LED shows a luminance of 9083 cd m-2, 3.36% external quantum efficiency (EQE), and 96% photoluminescence quantum yield (PLQY) efficiency (for the undoped CsPbBr3 LED, luminance: 844 cd m-2/EQE: 1.93%/PLQY: 85%). The LED based on 5%-doped Cs4PbBr6 shows a luminance of 11 440 cd m-2, an EQE of 6.27%, and 99% PLQY efficiency (for the undoped Cs4PbBr6 LED, luminance:1113 cd m-2/EQE: 1.64%/PLQY: 93%). It is expected that the results of this research will contribute to the perovskite LED research performed by thermal evaporation in the future.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call