Abstract

Single crystals of Sr 2 Ta 2 O 7 and Sr 2 Nb 2 O 7 are grown by a floating zone technique. Strontium tantalate belongs to D 2 h 14 or D 2 h 17 space group at room temperature. Ferroelectric phase transition temperature is -107°C. The Curie-Weiss temperature θ 0 and the Curie constant C P are: θ 0 =161 K(=-112°C) and C P =0.84×10 5 K. Spontaneous polarization and coercive field are 1.9 µC/cm 2 and 0.4 kV/cm at -190°C, respectively. Strontium niobate belongs to C 2υ 12 space group at room temperature. Its ferroelectric phase transition occurs at T c =1342±2°C, with θ 0 = T c and C P =1.2×10 5 K, and second phase transition occurs at -156°C. Solid solution Sr 2 (Ta 1- x ·Nb x ) 2 O 7 exists in the entire composition range and its ferroelectric phase transition temperature increases markedly from -107°C to 1342°C, according to the increase of x . Phase transition temperatures of other solid solutions, partially replacing Sr by Ca, Pb or Ba, are also studied on ceramic samples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call