Abstract
ABSTRACTInvestigation of crystallization behavior and kinetics of thermoplastic elastomer nanocomposites was the subject of limited works because of complexities associated with semiexperimental modeling of such phenomenon in a system containing components having completely different behavior in the molten state. Nonisothermal crystallization kinetics of dynamically vulcanized PA6/NBR/HNTs thermoplastic elastomer nanocomposites was mathematically modeled applying well‐known Avrami, Ozawa, and Mo theoretical models to the differential scanning calorimetry data gathered at various cooling rates. It was found that HNTs contribute as nucleating agents to the crystallization kinetics and cause acceleration of crystallization. Activation energy of the crystallization was calculated by correlating the crystallization peak temperature with the cooling rate using Kissinger model. It was found that Mo equation could properly describe nonisothermal crystallization kinetics of the PA6/NBR/HNTs thermoplastic elastomer nanocomposites. This was recognized from the obtained parameters of Mo equation in terms of HNTs loading level, which suggested a higher rate for dynamic crystallization. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018, 135, 46488.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.