Abstract

Amorphous structures of the as-cast bulk metallic glass samples (BMGs) of Cu60Zr25Ti15 and (Cu60Zr25Ti15)95Ni5 alloys are confirmed by X-ray diffraction. Isothermal crystallization kinetics of these BMGs are investigated using differential scanning calorimetry. For both the alloys, the apparent activation energy (Ea) shows a strong dependency on crystallization volume fraction (x). Isothermal crystallization kinetic parameters are calculated by Arrhenius and Johnson–Mehl–Avrami equations. Avrami exponential factor (n) is also found to show clear correlation with the crystallization volume fraction (x). It is found that the crystallization process is easier in Cu60Zr25Ti15 BMG than in (Cu60Zr25Ti15)95Ni5 BMG as the Ea decreases constantly for the former alloy though in the case of second alloy, the Ea is almost unchanged up to x = 60%. For both the alloys, nucleation activation energy (Enucleation) is found to be higher than that of growth activation energy (Egrowth). This indicates that the growth of crystals during isothermal crystallization in these glasses is easier than nucleation, and the minor addition of Ni causes the higher thermal stability against crystallization in isothermal condition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.