Abstract

Crystallization kinetics and structure of (85TeO2 + 15TiO2) and (85TeO2 + 10TiO3 + 5Fe2O3) glasses are studied using differential scanning calorimetry DSC, IR spectroscopy and XRD. DSC curves in the temperature range from 50 to 525°C with different heating rates from 10 to 40°C/min are used to study the crystallization behavior of the glasses and effects of different heating rates on the glass transition and crystallization temperatures (Tg and Tp). The activation energies of the glass transition and crystallization processes were determined from the shift of Tg and Tp with the heating rates using Kissinger's formula. Effects of the polymorphic nature of TeO2 on the crystallization mechanisms are discussed and the phases crystallized during the DSC process were identified by XRD. IR spectra in the frequency range (500–4000 cm-1 ) are measured and possible coordination states of the constituent oxides are discussed for heat-treated and untreated glasses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.