Abstract

The amorphous formation ability, crystallization behavior and magnetic properties of SmCo7 magnets melt-spun at 30 and 40 m/s have been studied. The ribbons melt-spun at 40 m/s exhibit amorphous structure in the range of 0.15x0.25 for SmCo7-x(Cr3C2)x alloys. In the amorphous state, these alloys are soft magnetic with intrinsic coercive field iHc of the order of 40-70 Oe. After annealing at 750 °C for 5 min, the alloy shows enhenced magnetic properties with iHc of 7.98 kOe, Mr of 55.05 emu/g, and Mr of 70.99 emu/g. The MFM image reveals a uniform distribution of individual grains with average size about 20 nm and a domain size about 100250 nm in width. This interaction domain results in the enhancement of the magnetic properties.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.