Abstract

The dielectric and crystalline properties of ferroelectric thin films of 0.9[Pb(Mg/sub 1/3/Nb/sub 2/3/)O/sub 3/]-0.1PbTiO/sub 3/ (.9PMN-.1PT) have been investigated. Ceramic targets of 0.9PMN-0.1PT with and without excess PbO were used for thin film deposition and were grown on substrates of SrTiO/sub 3/ LaAlO/sub 3/, MgO, and Pt/TiO/sub 2//SiO/sub 2//Si using pulsed laser ablation deposition. It was shown that the phase purity of the films was dependent on the film thickness. Furthermore we have shown that as the thickness of the films increases from 100nm to 600nm there is a progressive decline in the local strain and hence an improvement in the local crystallinity of the films. The dielectric constant for our films (3900 at 10KHz) is higher than previous reports on 0.9PMN-0.1PT films. We have also shown that there is considerable benefit in changing lower electrodes. The XRD shows that the films are highly c-axis orientated as grown on YBa/sub 2/Cu/sub 3/O/sub 7/ (001) or SrRuO/sub 3/ (001) and (111) orientated on Pt(111) lower electrodes. The sizes of the grains depend upon the nucleation density and the rate of growth onto the lower electrode used. Slower growth rates lead to excess of lead in the film at the grain boundaries while accelerated growth rates lead to higher porosity's. It was shown that annealing for 1 hour at 600/spl deg/C reduces porosity and improves surface quality.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.