In the title compound, C25H25NO7S, the mol-ecular conformation is stabilized by intra-molecular O-H⋯O and N-H⋯O hydrogen bonds, which form S(6) and S(8) ring motifs, respectively. The mol-ecules are bent at the S atom with a C-SO2-NH-C torsion angle of -70.86 (11)°. In the crystal, mol-ecules are linked by C-H⋯O and N-H⋯O hydrogen bonds, forming mol-ecular layers parallel to the (100) plane. C-H⋯π inter-actions are observed between these layers.