AbstractAqueous Zn‐ion batteries have emerged as promising candidates for large‐scale energy storage owing to their high safety and low cost. However, dendrite growth and side reactions compromise the stability of the Zn anode in practical applications. Here, a novel Zn anode featuring well‐designed crystal steps along the (002) facets, referred to as Step‐Zn is introduced. The intersections of the (002) and (100) planes in these crystal steps create preferential adsorption sites for Zn2⁺ ions, promoting initial electro‐epitaxial growth of Zn that uniformly covers the crystal steps. This process effectively regulates subsequent Zn deposition, ensuring fast reaction kinetics and smooth morphology without dendrite formation. Consequently, the unique Step‐Zn anode exhibits excellent cycle life over 6000 times at 3 mA cm−2 and low greatly reduced polarization voltage under high areal currents and capacities. Integrated with activated carbon (AC) cathode, the Step‐Zn||AC full cell demonstrates excellent durability over 10 000 cycles at 5 A g−1. This work offers valuable insights into controlling Zn deposition modes by engineering the surface microstructure of Zn anodes with greatly extended cycling stability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.