Abstract
Bulk single crystals of Sr3BeB6O13 with dimensions up to 50 × 30 × 5 mm3 were grown for the first time by a top-seeded solution growth method using H3BO3-LiF-SrF2 as flux. The average thermal expansion coefficients along the a-, b- and c-axis from 50 °C to 500 °C were determined as αa = 9.18 × 10−6 K−1, αb = 14.63 × 10−6 K−1, αc = 8.56 × 10−6 K−1, respectively. The specific heat was measured to be 0.771–0.844 J/(g·K) over the temperature range of 50–500 °C. In addition, the UV cutoff wavelength of Sr3BeB6O13 is located at 190 nm. Its refractive indices were accurately measured by a minimal deviation method, based on which the Sellmeier equations were derived.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.