Abstract

This paper reports the crystal growth and spectral properties of Nd 3+:Sr 2La 0.667(VO 4) 2 crystals. Nd:Sr 2La 0.667(VO 4) 2 crystal with dimension 20×15×15 mm 3 was grown by the Czochralski method. The segregation coefficients of Nd 3+ in Nd 3+:Sr 2La 0.667(VO 4) 2 crystal is 0.52. The hardness of Nd 3+:Sr 2La 0.667(VO 4) 2 crystal is 374.6 VDH, and is about equal to 5.0 moh. Nd:Sr 2La 0.667(VO 4) 2 crystal has a large FWHM of 21 nm at 810 nm. The absorption and emission cross-sections were 2.6×10 −20 cm 2 at 810 nm and 16.4×10 −20 cm 2 at 1079 nm, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.