Abstract
Ce:LiSrAlF6 and Eu:LiSrAlF6 crystals with different dopant concentrations were grown by the micro-pulling-down method. The crystals with high dopant crystal included the secondary phase as clusters with the plate shape in BSE images. The secondary phases were identified CeF3 and EuF2, respectively, by the EDS analysis and powder-XRD measurement. Eu concentration against the Sr sites in the Eu 2% doped LiSAF crystal were most uniform in the range 0.9–1.6atm% using the EPMA.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.