The crystal and magnetic structure of TbNiSnD has been studied by neutron powder diffraction. The deuteride crystallizes with the filled TiNiSi type structure (sp. gr. Pnma; a=7.0354(1); b=4.20662(9); c=8.1808(2) Å at 293 K; a=7.008(1); b=4.1954(6); c=8.153(1) Å at 2 K) and is canted ferromagnetic below 10 K. The deuterium atoms occupy the tetrahedral Tb 3Ni sites. The Tb atoms carry a magnetic moment of 6.6(1) μ B /Tb. They order antiferromagnetically along the a-axis and ferromagnetically along the c-axis. No significant magnetic moment on the Ni atoms has been observed by neutron diffraction. Insertion of deuterium in TbNiSn induces both a change of the magnetic structure and a reduction of the Tb magnitude of the magnetic moment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.