The effect of cryogenic treatment on mechanical properties and wear resistance at room temperature of 06Cr19Ni10 austenitic stainless steel was studied in the present study. The cryogenic treatment process was carried out at-160 and different time in program-controlled cryogenic container. The results showed that, after cryogenic treatment, the room-temperature mechanical properties of the 06Cr19Ni10 steel remained stable without embrittlement, friction coefficient of the 06Cr19Ni10 steel decreased and the wear resistance improved after cryogenic treatment. When cryogenic treatment was treated at-160 for two hours and thirty minutes, the friction coefficient of the 06Cr19Ni10 steel was the smallest and wear resistance was the best.