Abstract

Transmission electron microscopy in its modern high-resolution analytical form has great potential for elucidating mechanisms of environmental cracking in structural alloys and other materials. Apart from a few pioneering efforts, the difficulties of preparing suitable samples with the original corrosion structures preserved in narrow crack tips have limited contributions of TEM in this area. Recent work involving cross-sectional crack preparation has focused on intergranular stress-corrosion cracking of Fe- and Ni-base stainless alloys in high-temperature water. This presentation will illustrate preparation methods that have proven successful, and describe limitations of the analysis.The method for preparing cross-section samples suitable for high-resolution TEM characterization is based on earlier work by Lewis et al. It involves preparing a thin section containing cracks filled with epoxy, dimple grinding selected locations near the crack tip, and ion milling. Figure 1 schematically illustrates this method. The first step is to preserve the crack opening characteristics present under loading and protect the crack surfaces during thinning.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.