Abstract
Healing of critical-size defects is a well-known problem that has been challenged in several studies. The aim of the experiment was to evaluate bone formation and osseointegration of implants installed in critical defects of the mandibular body simultaneously grafted with Bio-Oss® or Cerabone®. Defects, 10mm wide and 3mm deep, were prepared at both lateral aspects of the mandible in 12 rabbits. One implant was installed in the center of the defect, and bovine xenografts produced either at low (Bio-Oss®; Low-T) or high (Cerabone®; High-T) temperatures were used to fill the defects. A collagen membrane was placed to cover the sites. Healing was evaluated 10weeks after surgery. In both groups, most sites showed optimal healing with closure of the coronal entrance of the defects. However, residual defects occupied by soft tissues and biomaterial particles were observed, even though generally limited to some regions of the defect. Osseointegration of the implant surface in the region of the defect was poor in both groups. Circumferential marginal critical-size defects around implants filled with bovine xenografts presented regions with a complete healing in both groups. However, the healing was not complete at all regions in most defects; therefore, a complete optimal healing of critical-size marginal defects cannot be predicted.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.