Long precursor filaments are prepared by dry spinning with a starting homogeneous aqueous PVA solution containing Y, Ba and Cu acetates. By controlling the spinning process and partial-melting, a high J c value of more than 10 5 A/cm 2 at 77 K and 0 T was obtained. The filament with high J c does not always have a texture well aligned to the direction of the fiber axis. The field dependence of the transport J c of the filament at 77 K is small if the grain boundary is clean.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.