Abstract

This paper reports on the microstructure-creep property relationship of three precipitation-strengthened tin (Sn)-based lead (Pb)-free solder alloys (Sn-0.7Cu, Sn-3.5Ag, and Sn-3.8Ag-0.7Cu) in bulk samples, together with Sn-37Pb as the alloy for comparison at temperatures of 303 K, 348 K, and 393 K. The creep resistance of these three Sn-based Pb-free solders increases, i.e., the steady-state creep rates decrease, with increasing volume fraction of precipitate phases for the Pb-free solder alloys. Their apparent stress exponents (na ∼ 7.3-17), which are all higher than that of pure Sn, attain higher values with increasing volume fraction of precipitate phases at constant temperature, and with decreasing temperature for the same solder alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.