Abstract

In this research work, the creep of thick-walled cylindrical vessels made of FGM with autofrettaged-treated was investigated using the analytical method. At different plastic depths and a variety of internal pressures for elastic modulus and yield stress constants ( n1 and n4), changes in residual creep strain rate (radial and circumferential) and final creep strain rate are investigated. The obtained results show that the circumferential stresses in the autofrettage have different values depending on the depth of the plastic. In the equivalent stress diagram, the resulting stress at the plastic points of the vessel reaches the yield stress of the FGM, and the stress decreases along the radius. If [Formula: see text] is increased from 1 to 1.8, the maximum creep strain rate decreases (for several n4, the dimensionless plastic depth is equal to 1.8). The results show that up to a dimensionless plastic depth of 1.5, the change in residual strain rate is negligible. The slope of the graphs for the dimensionless depths above 1.6 increases sharply. A comparison of the maximum circumferential stress as a function of plastic depth for the present work and the study by Darijani shows very good agreement between the two studies.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.