Eliminating hot cracking and achieving a good strength-ductility synergy in selective laser melted (SLMed) high-strength aluminium alloys remain challenging. We here inoculated 7050 high-strength aluminium alloy with 2 wt% Ti nanoparticles to eliminate hot cracking during SLM. Furthermore, ultrafine equiaxed grains with random textures were achieved in SLMed 7050 – 2 wt% Ti alloy, in contrast to the textured columnar grains observed in SLMed 7050 alloy. A high tensile yield strength of 393 MPa and an elongation of 11.6 % were achieved in SLMed 7050 – 2 wt% Ti alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.