Abstract

In this study environmental scanning electron microscopy was used to observe the cracking of drying latex films below their glass-transition temperature. By controlling the relative humidity so that it decreases linearly with time, a critical level of humidity at which cracking occurs can be determined and this is measured as a function of film thickness. It was found that the cracking humidity decreases with increases in film thickness for thicknesses in the range of 30 to 100 mum and then remains almost unchanged. A scaling argument can be used to fit the data very well and indicates that cracking occurs as soon as the entire film is consolidated into close packing.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.