The capacity of pure LiFePO 4 faded gradually from initial 149 mAh g −1–117 mAh g −1 under current density of 30 mA g −1 at room temperature after 60 cycles. Some obvious cracks are observed in LiFePO 4 particles after cycling. The formation of cracks would lead to poor electric contact and capacity fading. A possible mechanism is proposed for the appearance of the cracks.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.