Abstract

Crack initiation and propagation in creep-fatigue test were observed on semi-circular notched plates at elevated temperature by the CCD video camera. Test specimens are made of SUS304 stainless steel, and temperature is kept to be 550°C, and geometry of the semi-circular plate specimens are changed by diameter size of the hole. Photographs of all cycles were recorded to investigate crack initiation process in structural component having stress concentration and obtain number of cycle of crack initiation (Nc). The test results were compared with predictions by the Stress Redistribution Locus (SRL) method and the Neuber’s rule’s method.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.