Abstract

A new precipitation strengthening NiCoCr-based superalloy with favorable mechanical performance and corrosion resistance was designed for ultra-supercritical power generation equipment. The degradation of mechanical properties and steam corrosion at high temperatures put forward higher requirements for alternative alloy materials; however, when the superalloy is processed to form complex shaped components through advanced additive manufacturing techniques such as laser metal deposition (LMD), hot cracks are prone to appear. This study proposed that microcracks in LMD alloys could be alleviated with powder decorated by Y2O3 nanoparticles. The results show that adding 0.5 wt.% Y2O3 can refine grains significantly. The increase in grain boundaries makes the residual thermal stress more uniform to reduces the risk of hot cracking. In addition, the addition of Y2O3 nanoparticles enhanced the ultimate tensile strength of the superalloy at room temperature by 18.3% compared to original superalloy. The corrosion resistance was also improved with 0.5 wt.% Y2O3, which was attributed to the reduction of defects and the addition of inert nanoparticles.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.