Abstract

This review examines the different types of internal and surface cracks that can form during the continuous casting of steel. For each crack type, the operating and metallurgical factors that are known to influence crack formation are assessed in the light of the high temperature mechanical properties of steel and a knowledge of the stresses generated in the solidifying shell. The importance of two zones of low ductility in steel is demonstrated by this approach. One zone exists above 1340°C and probably accounts for the formation of all internal cracks and surface longitudinal cracks. The other zone lies between 700 and 900°C and is related to the presence of soluble aluminum, niobium and vanadium. Transverse surface cracks in slabs can be related to the latter zone.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.