Cr3C2 and VC doped WC–10wt.% Si3N4 composites were prepared by spark plasma sintering. The influences of Cr3C2 and VC on densification behavior, grain growth and mechanical properties of the WC–Si3N4 composites were investigated. During densification of the WC-based materials, the Cr3C2 and VC additives assist the preliminary densification of solid-state-sintering, and mitigate the subsequent densification of liquid-sintering. The addition of Cr3C2 and VC shows an inhibitory effect against WC-grain growth, resulting in higher hardness for the WC–Si3N4 composites. Moreover, the inhibitors do not hinder the transformation of α to β-Si3N4 and the growth of elongated β-Si3N4 grains, which act as toughening agent for the composites.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.