AbstractIn the context of growing interest in phosphonic acid proton exchange membranes (PEMs) for fuel cell applications, we report on new PEMs containing low‐cost polyethylene oxide (PEO) covalently linked by siloxane bonds, SiOSi, to phosphonic acid (PA). Key chemistry in the formation of these membranes involves hydrolysis and condensation reactions of triethoxysilyl propyl capped PEO and pre‐hydrolyzed dimethyl phosphonatoethyltrimethoxysilane (DMPTMS) giving PEO‐Si2O3‐PA and cross‐linked chain PEO‐Si2O3‐PEO organosilsesquioxane components. The Si2O3 can enhance membrane thermal and mechanical properties. The membrane formulations were varied by (a) reagent ratios (b) PEO molecular weights or using polypropylene oxide (PPO) (c) incorporating chain extending groups methylene diphenyl diisocyanate (MDI) or hexamethylene diisocyanate (HDI). These variations provided five membrane families, one of which afforded a complete group of robust membranes with weight% x of PA, PAx in range PA0–PA33. These were studied using ATR‐FTIR, dry membrane water uptake capacity, ion exchange capacity (IEC), and conductivity from room temperature to 120°C at 100% relative humidity. Conductivity increased with PAx reaching 15 mS cm−1 at 120°C, activation energy 0.1 eV, for membrane PA33 for which thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), scanning electron microscopy (SEM), and energy dispersive X‐ray analysis (EDAX) are reported. A comparative performance of the five membrane families is presented.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call