Abstract

Titanium alloys are popular metallic implant materials for use in total hip replacements. Although, α+β titanium alloys such as Ti-6Al-4V have been the most commonly used alloys, the high Young’s modulus (∼110GPa) leads to an undesirable stress shielding effect. An alternative is to use β titanium alloys that exhibit a significantly lower Young’s modulus (∼70GPa).Femoral stems made of a β titanium alloy known as TMZF (Ti-12Mo-6Zr-2Fe (wt.%)) have been used as part of modular hip replacements since the early 2000’s but these were recalled in 2011 by the US Food & Drug Administration (FDA) due to unacceptable levels of ‘wear debris’. The wear was caused by small relative movement of the stem and neck at the junction where they fit together in the modular hip replacement design. In this study, the corrosion and wear properties of the TMZF alloy were investigated in simulated body fluid to identify the reason for the wear debris generation. Ti64 was used as a control for comparison. It is shown that the interaction between the surfaces of Ti64 and TMZF with simulated body fluid is very similar, both from the point of view of the products formed and the kinetics of the reaction. The dry wear behaviour of TMZF is also close to that of Ti64 and consistent with expectations based on Archard’s law for abrasive wear. However, wear of Ti64 and TMZF in simulated body fluid show contrasting behaviours. A type of time-dependent wear test is used to examine the synergy between corrosion and wear of TMZF and Ti64. It is shown that the wear of TMZF accelerated rapidly in SBF whereas that of Ti64 is reduced. The critical role of the strain hardening capacity of the two materials and its role in helping the surface resist abrasion by hydroxyapatite particles formed as a result of the reaction with the SBF is discussed and recommendations are made for modifications that could be made to the TMZF alloy to improve the corrosion-wear response. Statement of SignificanceTMZF is a low modulus β-Ti alloy that has been used as the femoral stem in the Stryker modular design total hip replacement. It went into service in the early 2000’s but was recalled by the FDA in 2011 due to unacceptable levels of wear debris released in the body which led to adverse physiological reactions. A large number of these implants remain in patients today.In this contribution, we investigate the corrosion (interaction of the alloy with simulated body fluid (SBF)), dry wear and then corrosion-wear in SBF to identify the origin of the unacceptable levels of wear that led to the FDA recall of this material. We use Ti-6Al-4V as a control and demonstrate that the reaction between Ti64 and TMZF with SBF is very similar in terms of both products formed and kinetics. We also show that the dry wear behaviour of TMZF is very similar to that of Ti64 and exactly as should be expected for the hardness of this material.However, the wear behaviours of TMZF and Ti64 are completed different in SBF and wear of TMZF is significantly accelerated in SBF. A type of time-dependent wear test is used to demonstrate the synergy between corrosion and wear and the key role of the strain hardening capacity (or lack thereof in the case of β-Ti) is discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.