Abstract

The corrosion resistance of oxidized and nitrided commercially pure titanium obtained by sintering of powders of titanium, titanium hydride and their mixtures was evaluated in 20% aqueous solution of hydrochloric acid and 40% aqueous solution of sulfuric acid. It was determined that surface oxide film decreased the corrosion rate by three orders of magnitude for titanium obtained by powder metallurgy, and by one order for titanium obtained by deformation technology. In the absence of a surface film at oxidation of the sintered titanium, the corrosion rate decreased by 1–2 orders of magnitude compared to untreated titanium. It was shown that stage nitriding led to decrease in corrosion rate by 3–4 orders of magnitude for titanium obtained by both technologies.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.