Abstract

This work presents the influence of the surface treatment and plastic strain of Cr-Ni-Mo stainless steel, intended for implants applied in urogenital surgery, on the steel's corrosion resistance. Tests were carried out in simulated urine at a temperature of 37 1C and pH = 66,4. In particular, pitting and crevice corrosion resistance tests were carried out. Furthermore, through the applied technique of stent implantation, the deformability of the passive layer was evaluated. The deformability tests of the passive layer were carried out with the use of a bend test followed by a corrosion test.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.