Corrosion of the Fe–25Ni–15Cr superalloy under the combined effects of marine atmospheric exposure and high-temperature oxidation
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
https://doi.org/10.1016/j.matchar.2023.112885
Copy DOIJournal: Materials Characterization | Publication Date: Jul 1, 2023 |
Citations: 3 | License type: cc-by |
Corrosion of the Fe–25Ni–15Cr superalloy under the combined effects of marine atmospheric exposure and high-temperature oxidation