ABSTRACTThe corrosion behaviour of Magnox Waste (MW) glass in deionized water has been investigated under the aegis of the Japanese-Swedish-Swiss (JSS) project. The studies carried out at PSI and BNFL included static leaching and corrosion layer characterization. The results were used by HMI to derive the modelling parameters for the MW glass with the PHREEQE/GLASSOL codes. The silica concentration was found to strongly influence the corrosion rate of the glass. The MW glass selectively retains Cs due to the formation of a Cs-Mg-Al-Si-O-rich layer on its surface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.