Abstract

TiSiN thin films were deposited on NiCr dental alloy in order to enhance the corrosion resistance in artificial saliva with and without fluoride content. The TiSiN films were prepared using reactive cathodic arc method at two different substrate bias voltages (-50 V and-200 V). For the corrosion evaluation, artificial saliva with pH=5.2 was chosen, because this is a critical value for mineral dissolution of dental tissue which can affect the dental alloys. A content of 0.1 % NaF was added to the artificial saliva to simulate the effect of fluoride based hygiene products. The TiSiN coated NiCr alloys exhibited a higher corrosion resistance than the NiCr substrate, irrespective of the testing environment. The best corrosion resistance was found for the TiSiN deposited at-200 V.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.