Abstract

Corrosion behavior of extruded Mg, extruded AZ31 alloy, and cast AZ91 alloy was investigated by electrochemical measurements in dilute NaCl solutions. Corrosion products and passivation films were analyzed by X-ray diffraction and X-ray photoelectron spectroscopy. All specimens exhibit the corrosion and passivation zones in dilute NaCl solutions. The aluminum content and alloy microstructure influence the corrosion and passivation processes. AZ91 alloy shows the broadest passivation zone followed by AZ31 alloy and Mg. AZ91 alloy reveals a highest corrosion resistance, and preferential attack is located at the primary Mg phase. Its relatively fine β-phase (Mg17Al12) network and Al2O3/Al(OH)3 compounds produced on the passivation film are the main factors which limit the corrosion progress as compared with AZ31 alloy and Mg. The thick passivation product on AZ31 alloy is the key factor which restricts the corrosion attack in dilute solutions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.