Abstract
The aim of the present research was to investigate the role of the type of grain macrostructure (columnar, columnar-to-equiaxed transition–CET -, and equiaxed) and microstructure (secondary dendrite arm spacing - λ2) in the wear and electrochemical behavior of hypereutectic Zn–Al alloys (Zn-1wt%Al, Zn-2wt%Al, Zn-3wt%Al and Zn-4wt%Al) directionally solidified in a vertical upward directional solidification device. We also aimed to, correlate the thermal parameters with the electrochemical and wear properties. The results obtained in this alloy system indicate that the corrosion resistance decreases as the concentration of aluminum increases, but that at the highest concentrations (near the eutectic concentration) this resistance depends on the structure. For the same wear conditions, the wear rate of the equiaxed region is lower than the columnar and transition regions. Independently of the type of structure, wear resistance increases as the aluminum concentration increases.For each alloy concentration, the wear resistance increases from the columnar to the equiaxed structure. A clear inverse relation is observed between the wear resistance and λ2, which may explain the increase in wear resistance in the equiaxed region. At low spacings, the wear rate converges to a single value.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.