Abstract

Effects of microstructure on fracture toughness and transition temperature of high-toughness X70 pipeline steels were investigated in this study. Three types of steels were fabricated by varying alloying elements such as C, Cu, and Mo, and their microstructures were varied by rolling conditions such as finish rolling temperature and finish cooling temperature. Charpy V-notch (CVN) impact tests and pressed notch drop-weight tear tests (DWTT) were conducted on the rolled steel specimens. The Charpy impact test results indicated that the specimens rolled in the single-phase region of the steel containing a reduced amount of C and Mo had the highest upper shelf energy (USE) and the lowest energy transition temperature (ETT) because of the appropriate formation of acicular, quasipolygonal, or polygonal ferrite and the decreased fraction of martensite-austenite constituents. Most of the specimens rolled in the single-phase region also showed excellent DWTT properties as the percent shear area (pct SA) well exceeded 85 pct, irrespective of finish cooling temperatures, while their USE was higher than that of the specimens rolled in the two-phase region. Thus, overall fracture properties of the specimens rolled in the single-phase region were better than those of the specimens rolled in the two-phase region, considering both USE and pct SA.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.