Abstract: In the present work the effect of different durations of Post Weld Heat Treatment soaking times (0.5,2,10,50 hours) are analyzed on the mechanical and microstructural properties of Cr-Mo alloy steel of ASTM A387 Gr-22,2.25% Cr-1%Mo alloy steel. These are used in high temperature services in steam generation applications, Oil and Gas industries, Thermal and Nuclear power plants etc. The work is focused on different regions of weldment like base metal, HAZ and weld metal to compare and analyze the results obtained in as-welded and different soaking times from hardness test, tensile testing and microstructural examination. Results showed that the hardness varies from weld centre line to base metal and peak hardness was found in the HAZ. The hardness is reduced to large extent when PWHT is done at 50 h. Microstructural changes were observed during different post weld heat treatments and their effect on mechanical properties and best suitable soaking times were reported.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.