AlPO 4 -coated LiCoO 2 cathodes display improved cycle-life performance compared with bare LiCoO 2 . This is attributed to suppression of cobalt dissolution from the cathodes by the AlPO 4 -nanoparticle coating. Dissolution of cobalt during cycling with a charge cut-off voltage of 4.6 V leads to structural degradation, and induces a non-uniform distribution of local strain in the cathodes. The strain in coated samples is significantly reduced after 50 cycles, and is correlated with the enhanced cycle-life performance.